Research on pressure oxidation-iron alum decomposition-non-cyanide gold extraction of Carlin-type gold concentrate

  • English Author:
  • School of Metallurgy and Environment,Central South University|School of Metallurgy and Environment,Central South University&China Clean Metallurgy Engineering Research Center,China Nonferrous Metals Industry Association|School of Metallurgy and Environment,Central South University&China Clean Metallurgy Engineering Research Center,China Nonferrous Metals Industry Association|School of Metallurgy and Environment,Central South University&China Clean Metallurgy Engineering Research Center,China Nonferrous Metals Industry Association|School of Metallurgy and Environment,Central South University&China Clean Metallurgy Engineering Research Center,China Nonferrous Metals Industry Association|Zijin School of Geology and Mining,Fuzhou University
  • Unit:
  • PDF Download
  • Abstract
  • Online Preview
  • References

Abstract:

A Carlin-type gold concentrate is a typical refractory gold concentrate,and most of the gold is encapsulated in pyrite and arsenopyrite,with a gold leaching rate of only 7.8 % by direct leaching.In order to address the difficult gold extraction and severe pollution caused by cyanide leaching in Carlin-type gold concentrate,a gold extraction method using pressure oxidation-iron alum decomposition-non-cyanide gold extraction was proposed.The encapsulated gold can be effectively dissociated after pre-treatment by pressure oxidation and iron alum decomposition.The gold leaching rates of oxygen pressure residue and alum destruction slag were 76.2 % and 86.1 %,respectively,under the following conditions:reaction time of 2 h,activated carbon dosage of 50 g/L,stirring speed of 400 r/min,temperature of 30 ℃,pH value of 1.3-1.5,air flow rate of 2 L/min,liquid-solid ratio of 4∶1,and thiourea dosage of 4 g/L.This method realizes efficient and clean extraction of Carlin-type refractory gold concentrate.

Keywords:

Carlin-type gold concentrate;pressure oxidation;iron alum decomposition;non-cyanide gold extraction;encapsulated gold