福建某锌精矿铜钼综合回收试验研究

Experimental study on copper-molybdenum comprehensive recovery from a zinc concentrate in Fujian

  • 摘要: 福建某锌选矿厂的锌精矿含锌47.33%、含铜1.29%、含钼0.49%,铜、钼一直未得到有效回收。针对该锌精矿,开展再磨脱药—铜钼混合浮选—铜钼分离流程试验研究,铜钼混合浮选采用一粗两扫三精—粗精矿再磨工艺流程,铜钼分离采用一粗一扫四精工艺流程。全流程闭路试验可得到含铜20.11%、含金0.78 g/t、铜回收率65.9%的铜精矿,含钼39.49%、含铼18.28 g/t、钼回收率93.0%的钼精矿,以及含锌49.53%、锌回收率99.0%的锌精矿,有效降低了锌精矿中铜、钼杂质含量,同时得到了铜精矿和钼精矿产品,实现了锌、铜、钼的高效分离。

     

    Abstract: The zinc concentrate of a zinc beneficiation plant in Fujian contains 47.33% zinc, 1.29% copper, and 0.49% molybdenum, with copper and molybdenum not effectively recovered. For this zinc concentrate, experimental research was conducted using a regrinding and agent removal-copper and molybdenum mixed flotation-copper and molybdenum separation process. The copper and molybdenum mixed flotation process employed a rougher stage, two scavenging stages, and three cleaning stages, followed by regrinding of the rougher concentrate, while the copper and molybdenum separation process included a rougher stage, a scavenging stage, and four cleaning stages. The closed-circuit test of the entire process yielded a copper concentrate containing 20.11% copper and 0.78 g/t gold, with a copper recovery rate of 65.9%; a molybdenum concentrate containing 39.49% molybdenum and 18.28 g/t rhenium, with a molybdenum recovery rate of 93.0%; and a zinc concentrate containing 49.53% zinc, with a recovery rate of 99.0%. This effectively reduced the impurities of copper and molybdenum in the zinc concentrate, while obtaining high-quality copper and molybdenum concentrates, achieving efficient separation of zinc, copper, and molybdenum.

     

/

返回文章
返回